OHMALLOY COMPANY has a history of over fifty years in producing stainless steel. By selecting high quality raw materials and adopting melting processes of three-phase electroslag furnace+single-phase remelting funace, vacuum furnace,medium frequency induction furnace and electric arc furnace+vod furnace, the products are excellent in cleanliness and homogeneous、stable in composition. The series of Bar, wire can be provided.
Cold drawn wire Ф0.05-10.00mm
Steel bar Ф10.0-20.0mm
Chemical Composition of stainless steels:
Steel grades |
Chemical composition |
||||||||
C |
Si |
Mn |
Cr |
Ni |
Cu |
Mo |
N |
|
|
308 |
≤0.08 |
≤2.0 |
- |
19-21 |
10-12 |
- |
- |
|
|
309Nb |
≤0.08 |
≤1.0 |
≤2.0 |
22-24 |
12-16 |
- |
- |
|
|
316L |
≤0.03 |
≤1.0 |
≤2.0 |
16-18 |
10-14 |
- |
2-3 |
≤0.1 |
|
316Ti |
≤0.08 |
≤1.0 |
≤2.0 |
16-18 |
10-14 |
- |
2-3 |
≤0.1 |
Ti5(C+N)-0.7% |
304L |
≤0.03 |
≤1.0 |
≤2.0 |
18-20 |
8-12 |
- |
- |
≤0.1 |
|
800H |
≤0.05-0.1 |
≤1.0 |
≤1.5 |
19-23 |
30-35 |
≤0.75 |
- |
|
Fe≥39.5% Al:0.15-0.6 Ti:0.15-0.6 |
904L |
≤0.02 |
≤1.0 |
≤2.0 |
19-23 |
30-35 |
1-2 |
4-5 |
≤0.1 |
|
SUS430LX |
≤0.03 |
≤0.75 |
≤1.0 |
16-19 |
- |
- |
- |
- |
Ti/Nb0.1-1 |
SUS434 |
≤0.12 |
≤1.0 |
≤1.0 |
16-18 |
- |
- |
0.75-1.25 |
- |
|
329 |
≤0.08 |
≤0.75 |
≤1.0 |
23-28 |
2-5 |
- |
1-2 |
|
|
SUS630 |
≤0.07 |
≤1.0 |
≤1.0 |
15-17 |
3-5 |
3-5 |
- |
- |
Nb:0.05-0.35% |
SUS632 |
≤0.09 |
≤1.0 |
≤1.0 |
16-18 |
6.5-7.75 |
- |
- |
- |
Al:0.75-1.5 |
05Cr17Ni4Cu4Nb |
≤0.07 |
≤1.0 |
≤1.0 |
15-17.5 |
3-5 |
3-5 |
- |
- |
Nb:0.15-0.45% |